型號(hào): JH077 -[待選參數(shù)]

排氣栓

GASVEHT

不銹鋼——射出模具專用  硬度: RV50 孔徑: 0.05
stainless steel:special for ejection mold
 Hardness:RV50 Diameter:0.05
 銅---中空模具專用   硬度: RV20孔徑:0.35
 Copper:special for vacuumed mold
 Hardness:Rv20 Diameter:0.03

熱管方式之優(yōu)點(diǎn):

極微細(xì)的排氣孔,能將模具內(nèi)的瓦斯或空氣立即排出子模具外,簡(jiǎn)單而最有效果的産品爲(wèi)提升塑膠成型生産性能發(fā)揮威力.
     有效解決下列之間題:
     燒焦
     樹(shù)脂的填充較排氣快時(shí), 空氣受斷熱壓縮,前端部變成高溫,依情形而定, 會(huì)引起變色,燒焦等問(wèn)題。
     溢料
     在結(jié)合部前端的樹(shù)脂溫度上升,粘度下降,而易發(fā)生溢料,另外,空氣造成填充障礙,則射出壓力上升,結(jié)果模具微張,而全體發(fā)生溢料。
     填充不足
     雖然沒(méi)有燒焦、溢料發(fā)生,但因空氣造成的阻力,減緩了填充比率,造成填充不足的現(xiàn)象。
     氣泡銀線
     空氣與樹(shù)脂凝縮造成氣泡、銀線、污點(diǎn)等外觀不良問(wèn)題。
     循環(huán)時(shí)間延長(zhǎng)
     若提高樹(shù)脂溫度,模具溫度,降低射出速度,雖然這些不良現(xiàn)象不會(huì)發(fā)生,但使循環(huán)時(shí)問(wèn)延長(zhǎng)。
     節(jié)省能源、節(jié)省時(shí)間、節(jié)省成本
     若從設(shè)計(jì)階段開(kāi)始考慮TX排氣栓的話, 模具的試模次數(shù)、時(shí)問(wèn)、材料均可減少。
     裝入排氣栓的費(fèi)用與時(shí)間約以往的1/3-1/10。
     排氣栓使用方法:
     1.排氣栓在壓入模具時(shí),表面請(qǐng)勿直接打擊.
     2.排氣栓在壓入模具時(shí),請(qǐng)使用JIS規(guī)格H7/S6之公差。

In order to achieve its maximum molding productivities simply using its ultra micro breathing cell to      exhale gas and air from molds .
     Common Questions
     1.Burnt
     When aberration and burnt issues occurred,it is because resin is  filling faster than air exhaling      which will result  gasvent to overheat.
     2.0verflow:
     There are 2 possible conditions:
     When temperature of resin gets higher at the tip of seaming ,it weakens its bonding strength
     Air can  filled up the path and blocks resin to flow functionally which will cause ejection pressure      to rise  and  materials  to overflow.
     3.Not enough fillings:
     Due to air pressure ,it reduces the ratio of the filling speed. Even there is no any sign of burnt or overflow.
     4.Cell Streak:
     If there are some cells,streaks and mottles occurred ,it is because the cells  have not been      vaporized completely between air and resin.
     5.Extensive Cycling Time:
     The higher temperature of resin , molds and slower speed of injection cause extensive cycling time ,      however ,it will not affect the quality of final products.
     Energy,Time,and Cost Saver
     1.It will reduce the trial  die ,time and materials if users consider to use TX gasvent the beginning of the design.
     2.It will save up to 1/3 to 1/10 of the total cost and time if installing gasvent.
     Installation:
     1.Do not touch the surface when  gasvent is in use.
     2.Use H7/S6 from JIS reference chart.

Catalog No.LUSD
Type D
JH07744.51.55
5101.55
6101.55
8101.55
10101.55
12121.76
Order:Catalog No.DxL